3004 Aluminum Alloy Coil
Aluminum alloys have high ductility and corrosion resistance. The aluminum 3003 alloy has moderate strength and good corrosion resistance. The strength of this alloy can be increased by cold working.
Aluminium Grade: 3004
Width: 500~2600mm
Thickness: 0.2~12mm
Length: Coil
Temper: O, H111, H12, H22, H32, H14, H24, H34, H16, H26, H36, H18, H28, H38, H19, H112.
Certificate: ISO9001, CNAS, OHSAS18001
Packing: blank waterproof paper, kraft, wooden case or pallet (fumigation report for the wooden packing material)
Features: good formability, good workability, excellent corrosion resistance, and drawing characteristics
Overview of 3004 Aluminum Alloy Coil
Aluminium 3004 alloy is an alloy containing manganese and magnesium. The most widely used in buildings is the 3000 series “aluminium-manganese alloys,” of which the 3003, 3004, 3005, 3103 and 3105 alloys are used in large quantities, because the manganese content in the aluminium-manganese alloy is stable.
Features of 3004 Aluminum Alloy Coil
Like most other aluminum-manganese alloys, 3004 is a general-purpose alloy with medium strength, good workability and good corrosion resistance, always be made into the painted aluminum coil. It is usually rolled and extruded (used to make beverage cans), but it is usually not forged.
Applications of 3004 Aluminum Alloy Coil
It has many uses due to good strength, excellent corrosion resistance, good formability, good workability and drawing characteristics. This includes beverage cans, chemical equipment, hardware, storage tanks, and lamp bases.
Manufacturer of 3004 Aluminum Alloy Coil
Staral Alloy is a professional aluminum supplier, providing users with different types of aluminum products. The price of aluminium is not only low, but also has high corrosion resistance. We strictly control the production process of each product to ensure high quality.
Mechanical properties for 3004 Aluminum Alloy Coil
Properties | Metric | Imperial |
Tensile strength | 130 MPa | 18855 psi |
Yield strength | 125 MPa | 18130 psi |
Shear strength | 83 MPa | 12039 psi |
Fatigue strength | 55 MPa | 7977 psi |
Elastic modulus | 70-80 GPa | 10153-11603 ksi |
Poisson's ratio | 0.33 | 0.33 |
Elongation | 10% | 10% |
Hardness | 35 | 35 |
Chemical Composition of 3004 Aluminum Alloy Coil
Element | Content (%) |
Aluminum, Al | 98.6 |
Manganese, Mn | 1.2 |
Copper, Cu | 0.12 |